摘要
豫西某铅锌矿有用矿物共生关系密切、嵌布粒度较细,采用铅锌等可浮、铅锌分离-硫化锌浮选-氧化铅浮选工艺,成功实现了该矿的铅锌回收与分离,并有效回收了氧化铅矿物,最终获得了铅品位、回收率分别为58.95%、68.67%的铅精矿和锌品位、回收率分别为48.67%、66.06%的锌精矿。
Due to valuable minerals being closely-intergrown and finely-disseminated in a lead-zinc ore from west Henan, sequential processes including a Ph-Zn iso-flotation, a Pb/Zn separation, a zinc sulphide flotation and a lead oxide flotation were adopted to actualize recovery and separation of lead and zinc minerals, as well as efficient recovery of lead oxide minerals. This approach finally resulted in a lead concentrate approaching 58.95% Pb grade at 68.67% recovery, and a zinc concentrate grade of 48.67% Zn at 66.06% recovery.
出处
《矿冶工程》
CAS
CSCD
北大核心
2013年第6期36-37,41,共3页
Mining and Metallurgical Engineering
基金
中国国土资源部地质大调查项目(1212011120300)
关键词
浮选
铅锌矿
铅锌分离
氧化铅
flotation
lead/zinc ore
Pb/Zn separation
lead oxide