摘要
In this paper,the ammonia leaching process and high-energy ball milling method were adapted to recover spent LiCoO_(2) material.The ammonia reduction leaching mechanism of LiCoO_(2) material in the ammonia-sodium sulfite-ammonium chloride system was elucidated.Compared with untreated LiCoO_(2) material,the leaching equilibrium time of LiCoO_(2) after ball-milled for 5 h was reduced from 48 h to 4 h,and the leaching efficiency of lithium and cobalt was improved from 69.86%and 70.80%to 89.86%and98.22%,respectively.Importantly,the apparent activation energy and leaching kinetic equation of the reaction was calculated by the shrinking core reaction model,indicating that the reaction was controlled by the chemical reaction.
基金
financially supported by the National Natural Science Foundation of China(Nos.51822812,51778627)
the Fundamental Research Funds for the Central Universities of Central South University(No.2020zzts474)。