期刊文献+

帕娜碧亚F粘结系统在烤瓷贴面粘结中的应用 被引量:2

Clinical evaluation of Panavia F system on the bonding of porcelain veneer
在线阅读 下载PDF
导出
摘要 目的:通过对402颗烤瓷贴面的临床观察,评价帕娜碧亚F粘结系统对烤瓷贴面的粘结效果。方法:使用帕娜碧亚F粘结系统粘固402颗烤瓷贴面,观察6个月及12个月后贴面的密合性、脱落率和破损率等指标。结果:12个月后,贴面的脱落率及破损率低于1%,密合性好。结论:帕娜碧亚F粘结系统是一种较为理想的烤瓷贴面粘结材料。 Objective The purpose of this study was to evaluate the clinical results of 402 porcelain veneers bonded with the Panavia F system. Methods 402 porcelain veneers were bonded with Panavia F system in clinic. The restorations were recalled after 6 months and 12 months, respectively. Sealing capability, debonding and cataclasm were evaluated. Results After 12 months, less than 1% veneers were rebounded , no evident leakage was found. Conclusion Panavia F system is a reliable and ideal material for porcelain veneer bonding.
出处 《中国美容医学》 CAS 2005年第4期464-465,共2页 Chinese Journal of Aesthetic Medicine
关键词 烤瓷贴面 牙粘结技术 粘结剂 porcelain veneer dental bonding adhesive
  • 相关文献

参考文献5

  • 1陈吉华,施长溪,王玫,赵三军,王辉.546例四环素牙烤瓷贴面修复的临床观察[J].中华口腔医学杂志,2003,38(3):199-202. 被引量:55
  • 2王迎捷,陈吉华,赵桂文,王辉,何帅.不同偶联剂对瓷和树脂化学粘结的影响[J].口腔医学研究,2003,19(6):436-438. 被引量:11
  • 3Foxton RM, Pereira PN, Nakajima M, et al. Durability of the dual-cure resin cement/ceramic bond with different curing strategies[J]. J Adhes Dent, 2002, 4(1):49-59.
  • 4Dionysopoulos P, Kotsanos N, Pataridou A. Fluoride release and uptake by four new fluoride releasing restorative materials [J]. J Oral Rehabil,2003,30(9):866-872.
  • 5Tabassom Hooshmand,Richard van Noort, Alireza Keshvad, et al.Bond durability of the resin-bonded and silane treated ceramic surface[J]. Dent Mater, 2002, 18:179-188.

二级参考文献7

  • 1[1]Kato H,Matsumura H,Ide T,et al.Improved bonding of adhesive resin to sintered porcelain with the combination of acid etching and a two-liquid silane conditioner.J Oral Rehabil,2001,28∶102-108
  • 2[3]Chen JH,Matsumura H,Atsura M.Effect of etchant,etching period, and silane priming on bond strength to porcelain of composite resin.J Oper Dent,1998,23∶250-257
  • 3[4]Tabassom Hooshmand,Richard van Noort,Alireza Keshvad. Bond durability of the resin -bonded and silane treated ceramic surface.Dent Mat,2002,18∶179-188
  • 4[5]Hato H,Matsumura H,Tanaka T,et al.Bond strength and durability of porcelain bonding systems. J Prosthet Dent,1996,75∶163-168
  • 5[6]Sato K,Matsumura H ,Atsuta M.Effect of three-liquid bonding agents on bond strength to a machine milled ceramic material.J Oral Rehabil,1999,26∶570-574
  • 6[7]Molin MK,Karlsson SL,Kristiansen MS.Influence of film thickness on joint bond strength of a ceramic/resin composite joint.Dent Mat,1996,12∶245-252
  • 7曲晓莉,陈吉华,伊元夫.酸蚀及偶联剂的使用对瓷与树脂剪切粘结强度的影响[J].中国美容医学,1999,8(2):120-121. 被引量:6

共引文献64

同被引文献13

  • 1章利.一种正畸粘结材料反复粘结托槽的剪切强度研究[J].江西医药,2004,39(5):360-361. 被引量:1
  • 2袁元.直接粘结颊面管与带环颊面管在直丝弓矫治技术中的对比研究[J].临床口腔医学杂志,2007,23(4):231-232. 被引量:15
  • 3牛光良.瓷贴面粘接技术[J].口腔颌面修复学杂志,2013,14(1).
  • 4Gorucu J, Gurgan S, Cakir FY, et al. The effect of different prepara- tion and etching procedures on the mioroleakage of direct composite veneer restorations [J]. Photomedicine and Laser Surgery, 2011,29 (3) : 205-211.
  • 5Ozt~irk E,Bolay ~,Hickel R,et al. Shear bond strength of porcelain laminate veneers to enamel,dentine and enamel-dentine complex bonded with different a3hesive luting systems [J]. J Dent, 2013,41 (2) : 97-10S.
  • 6De Munck J, Van Meerbeek B, Yudhira R, et al. Micro-tensile bond strength of two adhesives to Erbium: YAG-lased vs. bur-cut enamel and dentin[J]. Eur J Oral Sci, 2002, 110 (4) : 322-329.
  • 7Bachm ann L, Die bolder R, Hibst R,et al. Changes in chemical composition and collagen structure of dentine tis sue after erbium laser irradiation [J]. Spectroch im Acta A Mol Biomol Spectrosc, 2005,61 (11-12) : 2634-2639.
  • 8Martinez-Insua A, Da Silva Domingez L, Rivera FG, et al. Differ- ences in bonding to acidetched or Er: YAG-lased-treated enamel and dentin surfaces [J].J. Prosthet. Dent, 2000, 84 (3):280-288.
  • 9Liberman R, Segal TH,Nordenberg D,et al. Adhesion of composite materials to enamel:comparison between the use of acid and lasing as pretreatment [J]. Lasers Surg. Med, 1984, 4 (4) : 323-327.
  • 10卢红飞.固定正畸治疗引起牙釉质脱矿的直接原因及其影响因素和预防方法[J].国际口腔医学杂志,2004,32(S1):167-169. 被引量:22

引证文献2

二级引证文献6

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部