摘要
针对某铁矿选厂尾矿中镜铁矿粗细嵌布不均的特点,采用重选-磁选-浮选和重选-磁选-重选工艺流程分别进行选别,分别获得了铁精矿产率22.26%、铁品位65.86%、铁回收率71.76%与铁精矿产率20.44%、铁品位66.13%、铁回收率66.16%的良好试验指标。研究成果不仅为该尾矿资源的开发利用提供了技术支撑,而且对同类二次资源的高效开发具有重要的指导和借鉴意义。
According to the characteristics of uneven size distribution of specularite particles in the tailings from some iron ore concentrator, experimental studies were performed by two flowsheets respectively. Results showed that a combined process of gravity separation-magnetic separation-flotation produced an iron concentrate approaching 65.86% Fe grade at 71.76% recovery with a yield of 22.26%, and another process of gravity separation-magnetic separationgravity separation led to an iron concentrate approaching 66.13% Fe grade at 66.16% recovery with a yield of 20.44%. This study can provide a technical reference and guidance not only for the exploitation of such kind of tailings, but also for the efficient utilization of secondary resources of this kind.
出处
《矿冶工程》
CAS
CSCD
北大核心
2014年第5期34-38,共5页
Mining and Metallurgical Engineering
基金
"十二五"国家科技支撑计划课题(2012BAB23G01)
关键词
二次资源
镜铁矿
重选
角闪石
正浮选
secondary resources
specularite
gravity separation
hornblende
direct flotation