摘要 The elevated temperature creep properties(90-150℃) of high silicon(~6wt%Si) alloy ZA27 prepared by spray deposition have been investigated by means of ball hardness testing method.The results indicate that the creep properties of the material prepared by spray deposition are notably improved,compared to that of the conventional casting alloy ZA27.The creep activation energy of the spray deposited alloy ZA27 is 3.9-5.7 kJ/mol higher than that of the conventional casting alloy ZA27.The creep formulation in this experiment is also derived as follows:HB-2-HB0-2=K exp(- Q/3RT)(t1/3-t01/3)The reasons for the improvement of creep resistance are also discussed from a microstructural point of view. The elevated temperature creep properties(90-150℃) of high silicon(~6wt%Si) alloy ZA27 prepared by spray deposition have been investigated by means of ball hardness testing method.The results indicate that the creep properties of the material prepared by spray deposition are notably improved,compared to that of the conventional casting alloy ZA27.The creep activation energy of the spray deposited alloy ZA27 is 3.9-5.7 kJ/mol higher than that of the conventional casting alloy ZA27.The creep formulation in this experiment is also derived as follows:HB-2-HB0-2=K exp(- Q/3RT)(t1/3-t01/3)The reasons for the improvement of creep resistance are also discussed from a microstructural point of view.
出处 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 1996年第2期140-146,共7页 金属学报(英文版)
关键词 spray deposition zinc-based alloy CREEP MICROSTRUCTURE spray deposition,zinc-based alloy,creep,microstructure
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部