摘要
目的研究牙科钛表面烤瓷烧结次数对钛烤瓷修复体颜色的影响,以指导技工和临床烤瓷操作,同时比较两种瓷粉的颜色在烧结中的稳定性能是否存在差异。方法采用Ti-22和Vita Titankeramik两种钛瓷粉,设计制作钛瓷标准试件,包括遮色瓷、体瓷和钛-遮色瓷-体瓷试件,经1、3、5、7、9次烧结处理,每次烧结后采用ShadeEye NCC比色仪,根据CIE1976L*a*b*色度系统标准测量各样本的L*a*b*值,并计算色差值、彩度和色调角,进行统计分析。结果烧结5次以内,各组试件的L*a*b*值及彩度、明度、色差及色调角均无明显变化,继续烧结后两种瓷粉的L*a*值均发生变化,且有统计学差异(P<0.05)。经过9次烧结,各组试件的色差变化均小于1.5。结论烧结次数在5次以内,钛瓷的颜色无明显变化,继续烧结则出现颜色差异,但肉眼尚未能辨别。
Objective To investigate the influence of repeated sintering on the color of two porcelain-fused-totitanium, and the differences between the two porcelains. Methods Thirty samples were prepared and sintered for 9 times. The color of samples were measured following sintering 1, 3, 5, 7, 9 times by ShadeEye NCC colodmeter according to two brands of porcelains with CIE1976L*a*b* color system, and calculated relevant chrome, chromatism and hue, and statistical analysis. Results When two brands of porcelains were sintered 5 times, the color parameters had no significant change and sintered continuely, the color parameters of L* and a* had obvious changes, but can't be observed by eyes. Conclusion The color parameters of titanium-porcelains have no significant change after repeated sintering.
出处
《华西口腔医学杂志》
CAS
CSCD
北大核心
2007年第4期354-357,共4页
West China Journal of Stomatology
基金
江苏省"135"重点人才基金资助项目(2002008)
关键词
烧结钛-瓷
颜色
烧结
色度计
porcelain-fused-to-titanium
color
sintering
colorimeter