再生水消毒对循环冷却水系统的腐蚀速率研究 被引量:5

Corrosion of Stainless Steel 316L in Disinfected Recycling Water
原文传递
导出
摘要 无机消毒剂Cl O2和有机消毒剂季铵盐(苯扎溴铵)作为常用的再生水消毒剂对循环冷却水系统具有一定的腐蚀性。通过两种消毒剂的对比,发现消毒后残留的Cl-和氨氮分别是两种消毒剂对316L不锈钢产生腐蚀的主要因素。此外,采用响应面分析法(RSM)和中心组合设计(CCD)分析了温度和流速对316L不锈钢腐蚀速率的作用。结果表明,在低温和低流速的情况下,瞬时腐蚀速率变化较小,产生腐蚀的主要原因还是电化学腐蚀。 As common disinfectant inorganic Cl O2 and organic quaternary ammonium salt(benzalkonium bromide) exhibits certain corrosivity for the facilities of the circulating cooling water system. Through a contrast test for the two kinds of disinfectant, it is found that Cl-and ammonia nitrogen respectively are the main factors responsible to the corrosion of 316 L stainless. In addition, the influence of temperature and water flow velocity on the corrosion rate of 316 L stainless steel was analyzed by means of response surface method(RSM) and central composite design(CCD). It follows that the instantaneous corrosion rate changes little at low temperature and low water flow velocity. And the main cause for corrosion is electrochemical corrosion.
出处 《腐蚀科学与防护技术》 CAS CSCD 北大核心 2015年第1期64-68,共5页 Corrosion Science and Protection Technology
基金 中央高校基本科研业务费专项资金资助
关键词 CLO2 季铵盐 腐蚀 再生水 chlorine dioxide,quaternary ammonium salt,corrosion,recycling water
  • 相关文献

参考文献15

二级参考文献120

共引文献211

同被引文献52

引证文献5

二级引证文献12

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部