Investigation of luminescence from SiC nano-granule films on porous glass substrate
1
作者 ZHEN Cong-mian ZHANG Jin-juan +3 位作者 WANG Xiao-qiang ZHANG Yong-jin PAN Cheng-fu HOU Deng-lu 《Optoelectronics Letters》 EI 2008年第6期429-432,共4页
SiC granule films were fabricated onto porous glass substrate by RF-magnetron sputtering. Photoluminescence (PL) measurements show that there are light emissions at three different wavelengths. Ultraviolet emission ... SiC granule films were fabricated onto porous glass substrate by RF-magnetron sputtering. Photoluminescence (PL) measurements show that there are light emissions at three different wavelengths. Ultraviolet emission peaked at 360 nm originated from the band-band transmission of SiC nanoparticles with relatively small size. The 370 nm light emission was due to the luminescence of the nano-skeletons of porous glass that was formed during the etching of the glass substrate. The blue emission at about 460 nm was associated with the recombination of the excited electron and O-deficient defects appeared at the interface between SiC nanoparticles and the porous glass. Furthermore, the optimal PL performance was obtained when SiC deposited time was I h and the glass substrate was etched for 20 min in the annealing sample (450 ℃). 展开更多
关键词 发光特征 sic 纳米颗粒薄膜 多孔渗水玻璃基底
在线阅读 下载PDF
热退火诱导C^+注入Si晶体的蓝光发射
2
作者 周原 王茺 +2 位作者 韦冬 卢赛 杨宇 《人工晶体学报》 EI CAS CSCD 北大核心 2014年第4期918-922,共5页
在室温和注入能量为60 keV的条件下,在硅晶片中注入C+,使其剂量达到5.0×1016cm-2,随后即对样品进行高温退火处理。采用X射线衍射(XRD),拉曼和光致发光(PL)光谱技术对样品进行了表征。实验结果显示:C+注入后经高温退火的样品的XRD... 在室温和注入能量为60 keV的条件下,在硅晶片中注入C+,使其剂量达到5.0×1016cm-2,随后即对样品进行高温退火处理。采用X射线衍射(XRD),拉曼和光致发光(PL)光谱技术对样品进行了表征。实验结果显示:C+注入后经高温退火的样品的XRD图谱中,在40°附近处出现了衍射峰,表明经退火后样品中形成了纳米尺寸的SiC团簇,并观察到了强烈的蓝光发射。PL光谱中的蓝光峰起源于量子限制效应。 展开更多
关键词 离子注入 sic发光 量子限制效应
在线阅读 下载PDF