含砷钴镍渣中砷碱介质氧化浸出机理 被引量:6
1
作者 余国林 张盈 +3 位作者 郑诗礼 邹兴 王晓辉 张懿 《过程工程学报》 CAS CSCD 北大核心 2013年第6期939-945,共7页
研究了某厂ZnSO4溶液砷盐净化工艺产生的含砷钴镍渣中砷在惰性和氧气气氛的碱介质中的氧化浸出机理.结果表明,砷氧化浸出与温度、介质碱浓度、浸出气氛均密切相关.在惰性气氛、碱介质中,渣中CuO和Cu2O均可作为砷氧化浸出的氧化剂,在80... 研究了某厂ZnSO4溶液砷盐净化工艺产生的含砷钴镍渣中砷在惰性和氧气气氛的碱介质中的氧化浸出机理.结果表明,砷氧化浸出与温度、介质碱浓度、浸出气氛均密切相关.在惰性气氛、碱介质中,渣中CuO和Cu2O均可作为砷氧化浸出的氧化剂,在80℃及以下低温下,CuO对低价砷起主要氧化作用,还原产物为Cu2O,砷最高浸出率不超过53%;在100℃及以上较高温下,CuO和Cu2O均参与低价砷的氧化浸出过程,还原产物均为单质Cu,最高浸出率约为90%;在氧气气氛、碱介质中,砷浸出率可达98%以上,除O2作为氧化剂直接氧化浸出砷外,渣中的铜可作为O2与低价砷之间电子传递的载体,强化氧化反应. 展开更多
关键词 含砷钴镍渣 碱介质 氧化 氧化浸出 机理
原文传递
Extraction of arsenic from arsenic-containing cobalt and nickel slag and preparation of arsenic-bearing compounds 被引量:12
2
作者 余国林 张盈 +3 位作者 郑诗礼 邹兴 王晓辉 张懿 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2014年第6期1918-1927,共10页
The arsenic extraction from the arsenic-containing cobalt and nickel slag,which came from the purification process of zinc sulfate solution in a zinc smelting factory,was investigated.The alkaline leaching method was ... The arsenic extraction from the arsenic-containing cobalt and nickel slag,which came from the purification process of zinc sulfate solution in a zinc smelting factory,was investigated.The alkaline leaching method was proposed according to the mode of occurrence of arsenic in the slag and its amphoteric characteristic.The leaching experiments were conducted in the alkaline aqueous medium,with bubbling of oxygen into the solution,and the optimal conditions for leaching arsenic were determined.The results showed that the extraction rate of arsenic was maximized at 99.10%under the optimal conditions of temperature 140 ℃,NaOH concentration 150 g/L,oxygen partial pressure 0.5 MPa,and a liquid-to-solid ratio 5:1.Based on the solubilities of As2O5,ZnO and PbO in NaOH solution at 25 ℃,a method for the separation of As in the form of sodium arsenate salt from the arsenic-rich leachate via cooling crystallization was established,and the reaction medium could be fully recycled.The crystallization rate was confirmed to reach 88.9%(calculated on the basis of Na3AsO4) upon a direct cooling of the hot leachate down to room temperature.On the basis of redox potentials,the sodium arsenate solution could be further reduced by sulfur dioxide(SO2) gas to arsenite,at a reduction yield of 92%under the suitable conditions.Arsenic trioxide with regular octahedron shape could be prepared successfully from the reduced solution,and further recycled to the purification process to purify the zinc sulfate solution.Also,sodium arsenite solution obtained after the reduction of arsenate could be directly used to purify the zinc sulfate solution.Therefore,the technical scheme of alkaline leaching with pressured oxygen,cooling crystallization,arsenate reduction by SO2 gas,and arsenic trioxide preparation,provides an attractive approach to realize the resource utilization of arsenic-containing cobalt and nickel slag. 展开更多
关键词 arsenic-containing cobalt and nickel slag alkaline leaching cooling crystallization sodium arsenate arsenic trioxide