The adsorption-desorption of silica nanoparticles(NPs) on poly(ethylene glycol)(PEG) grafted onto gold(Au) substrate was studied by quartz crystal microbalance with dissipation monitoring(QCM-D) technique. T...The adsorption-desorption of silica nanoparticles(NPs) on poly(ethylene glycol)(PEG) grafted onto gold(Au) substrate was studied by quartz crystal microbalance with dissipation monitoring(QCM-D) technique. The results of frequency and dissipation show that SiO2 NPs can be adsorbed strongly on PEG-SH brushes at pH of 9.6, and a new dense and rigid construction is formed. Adjusting the pH from 9.6 to 12.3 resulted in the desorption of si- lica NPs from the PEG brushes because of a significant weakening of the hydrogen bond between the silica NPs and PEG chains. In addition, the viscoelastic properties of the system during the adsorption-desorption process were also analyzed via the relationship between the normalized frequency(Af/n) and mass. And the corresponding atomic force microscopy(AFM) images also exhibit morphological changes during the above process, consistent with the changes in viscoelasticity.展开更多
基金Supported by the National Natural Science Foundation of China(Nos.50621302, 50921062).
文摘The adsorption-desorption of silica nanoparticles(NPs) on poly(ethylene glycol)(PEG) grafted onto gold(Au) substrate was studied by quartz crystal microbalance with dissipation monitoring(QCM-D) technique. The results of frequency and dissipation show that SiO2 NPs can be adsorbed strongly on PEG-SH brushes at pH of 9.6, and a new dense and rigid construction is formed. Adjusting the pH from 9.6 to 12.3 resulted in the desorption of si- lica NPs from the PEG brushes because of a significant weakening of the hydrogen bond between the silica NPs and PEG chains. In addition, the viscoelastic properties of the system during the adsorption-desorption process were also analyzed via the relationship between the normalized frequency(Af/n) and mass. And the corresponding atomic force microscopy(AFM) images also exhibit morphological changes during the above process, consistent with the changes in viscoelasticity.